I am sorry if this is the wrong forum for this but I am at my wits end. Can someone here direct me to, or provide, the following mechanical properties for A588 grade A steel?

Elastic Modulus
Poisson's Ratio
Shear Modulus
Density
Tensile Strength
Yield Strength
Thermal Expansion Coefficient
Thermal conductivity
Specific Heat

all I know is tensile/ultimate strength is around 100ksi and yield is around 50ksi. I can find any information anywhere on the other properties. I have read that the properties change depending on the size and shape. I am using plate less than 1" thick. Any help on this subject would greatly be appreciated.
 
Replies continue below

Recommended for you

The yield strength and tensile strength are specified in ASTM A 588, available from ASTM International at:


MatWeb has all but the last three:


And for those, you could use the values for 1020 steel:


Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thank you SO much. Was this the proper forum to post this question?
 
Yes

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 