Hi
I need ,metal paste for alluminium to fill the cut outs.
And after pasting metal,i need to send it to for chromating.

Is there any metal paste which will not go after chromating.

thanx in before

Jhon
 
Replies continue below

Recommended for you

you can use JB weld to fill small holes, but it will not plate, can be painted
otherwise dig out the tig welder and replace the metal

SBI
Central Ne.,USA
 
Thanx to sbi & goahead,
Problem by welding,component will break bz of heat
i need any cool process,which will satisfy my requirement

John
 
If possible:

Tap the holes.
Plug them with a shouldered plug that leaves less than 1/8 to a 1/16 of the shoulder above the top surface, use some locktite if possible to prevent the possiblity of it backing out in operation.
Peane the plug to fill and flow over the top thread.
Then machine the surface flush.

Odds are you will not ever be able to find the plugs if you do it correctly. I used to be a master at repairing booboos when I was a machinist it is an artform, I have never received a customer complaint on a reworked part.
 