Hi all,
We have a plastic (UHMWPE or nylon) wheel. It's 30mm in diameter, and only 4mm wide.
Want to measure the surface roughness across the 4mm face.
Does anyone know is it possible to measure surface roughness on plastics like that?
And across such a short distance while on a radius?
Thanks
CBecks
We have a plastic (UHMWPE or nylon) wheel. It's 30mm in diameter, and only 4mm wide.
Want to measure the surface roughness across the 4mm face.
Does anyone know is it possible to measure surface roughness on plastics like that?
And across such a short distance while on a radius?
Thanks
CBecks