Hi, I am looking for a type of tensometer (or something like that) to measure strain/deformation in a plastic housing caused by thermal expansion. According to a super straight-forward hand calculation the deflection at a given point will be 1.3mm. The temperature change is from 23 to 80 Celsius.
I have very little experience with this type of applications. I am more interested in a relative change in position between 2 points (distance is about 330mm) rather than the local strain in the material itself. What would you recommend?
I have very little experience with this type of applications. I am more interested in a relative change in position between 2 points (distance is about 330mm) rather than the local strain in the material itself. What would you recommend?