I have a 1-1/4" thick lifting lug that I'm welding to a 3/8" thick stiffened stack using a fillet weld. The weld is not located near a seam in the stack.
What is the maximum size fillet weld I can use for the lifting lug to stack connection? I've typically used 3/8" maximum for this based on the minimum material thickness, but, may need to go a little larger.
The material is 304L stainless and failure will be through the base metal and not the weld. The use of 3/8" has been for distortion and cracking control.
Dik
What is the maximum size fillet weld I can use for the lifting lug to stack connection? I've typically used 3/8" maximum for this based on the minimum material thickness, but, may need to go a little larger.
The material is 304L stainless and failure will be through the base metal and not the weld. The use of 3/8" has been for distortion and cracking control.
Dik