Does ASME Construction codes specially B31.1 and section I limit or provide reference to maximum number of PWHT cycles that can be carried out on circumferential welds of A106GrB?
 
Replies continue below

Recommended for you

No, there is no maximum limit provided the WPS/PQR is qualified with PWHT for non-impact qualification. For impact qualification, the maximum aggregate time is required.
 
While the Codes do not limit cycles, many Owners/Engineers specifications do.
 