When it comes to tolerances of the nominal thickness of a pipe, most pipespecs have this text:
"The minimum wall thickness at any point shall not be more than 12.5% under the nominal wall thickness specified."

So how much thicker than the nominal thickness is the pipe allowed to be?
 
Replies continue below

Recommended for you

Depends om material specification.
E.g. for A 312 see table 3. for plus tolerance.
 
Thanks Ijzer, does A 106 and A 335 have a similar table, can't seam to find one?

 
Look at the front page of your spec. It will refer you to others,your answer will be there.
 
Found it in A 530 Table 1, thx all.
 
In some pipe specs the max wall is only limited by the total weight of the pipe.
Yes, in most cases you can ship sch80 in place of sch40 and it meets the specs.
Got'a love pipe.

= = = = = = = = = = = = = = = = = = = =
Rust never sleeps
Neither should your protection
 