Hi,

Where do I find the minimum service temperature of materials?

I am looking specifically for AISI 316 SS, but I can’t seem to find it in the codes.

Thanks!
 
Which code? And which 316? EN 10216-5 1.4304 or ASTM A312 TP316/316L, or ... ?
 
For the ASME Boiler and Pressure Vessel Codes, review ASME Section II. For B31.3, review the Tables therein including the Notes. For other answer the questions of XL83NL.
 