Right could anyone help me with Secant Modulus at 2.5%, Specific strength, Specific tensile modulus
i.e. Secant Mod = Yield load/CSA * Gauge L/Delta L, does this seem like the right formula for secant at 2mm?
Gauge length for all materials: 80mm
Material:
Nylon 66, UF
Nylon 66, F
Polycarbonate (PC)
Polypropylene (PP)
Mild Steel
Aluminium
With respective density's:
1.14E+06
1.38E+06
1.20E+06
9.00E+05
7.90E+06
2.70E+06
For the CSA, is it correct to use the ORIGINAL CSA of the material?
Cheers
Mike
New on here!
Right could anyone help me with Secant Modulus at 2.5%, Specific strength, Specific tensile modulus
i.e. Secant Mod = Yield load/CSA * Gauge L/Delta L, does this seem like the right formula for secant at 2mm?
Gauge length for all materials: 80mm
Material:
Nylon 66, UF
Nylon 66, F
Polycarbonate (PC)
Polypropylene (PP)
Mild Steel
Aluminium
With respective density's:
1.14E+06
1.38E+06
1.20E+06
9.00E+05
7.90E+06
2.70E+06
For the CSA, is it correct to use the ORIGINAL CSA of the material?
Cheers