yesterday, during a material inspection, i got one spectacle blind for inspection. MTC was available for the spectacle blind and MTC was telling that it is A105 material. But there was no punching or any identification in the spectacle blind. So i recommended for PMI test and Hardness test to verify the material. The PMI report is as follows...
Fe----98.74
Zn----0.075
Mn----0.878
Hardness value observed to be 139-150BHN
Can i accept this material as A105 based on this PMI test?
yesterday, during a material inspection, i got one spectacle blind for inspection. MTC was available for the spectacle blind and MTC was telling that it is A105 material. But there was no punching or any identification in the spectacle blind. So i recommended for PMI test and Hardness test to verify the material. The PMI report is as follows...
Fe----98.74
Zn----0.075
Mn----0.878
Hardness value observed to be 139-150BHN
Can i accept this material as A105 based on this PMI test?