Hi all,
I have reviewed material test certificate (MTC) for steel flat bars conforming to ASTM A 36 where chemical composition and all mechanical properties are detailed and thus, meeting the requirements of A36.
Our concern is that EN 10204 3.1 is not mentioned in the MTC and client has raised the same query since it was required by their specification (MTC to EN 10204 3.1).
My question is “does it mandatory for manufacturer to mention in MTC as EN 10204 3.1 certified even though it meets international standard material grade properties” ??
Regards
I have reviewed material test certificate (MTC) for steel flat bars conforming to ASTM A 36 where chemical composition and all mechanical properties are detailed and thus, meeting the requirements of A36.
Our concern is that EN 10204 3.1 is not mentioned in the MTC and client has raised the same query since it was required by their specification (MTC to EN 10204 3.1).
My question is “does it mandatory for manufacturer to mention in MTC as EN 10204 3.1 certified even though it meets international standard material grade properties” ??
Regards