Hello

I need to work on some old vessels and require the allowable stresses of SA201-A at 100F and 825F and SA201-B at 100F and 500F, Can anyone help?

Thanks in advance

Tomtation
 
Replies continue below

Recommended for you

For SA-201 Grade A at 850 deg F the allowable is 7,800 psi. So, you can do the interpolation yourself. The 850 deg F is also when time dependent properties dominate.
 