Hi,

1)Can anybody supply me with the chemical composition and mechanical properties(Min Yield Strength for ASTM SA-350 Grade LF6 Class 1 and Class 2?

2)Can anybody supply me with the chemical composition for ASTM SA 358 309H,Gr.2.,ASTM SA 694,ASTM SA 242(Welding)
and ASTM SA 381? I also need the Minimum design temperatures(C)and Impact Test Requirements forthese material specs.

3)Can anybody supply me with the Minimum design temperatures(F/C)for the following material specifications:
ASTM A 182 F316H, Gr.2
ASTM A 182 F317, Gr.2
ASTM A 182 F317H, Gr.2
ASTM A 182 F44, Gr.2
ASTM A 182 F51, Gr.2
ASTM A 182 F53, Gr.2
ASTM A 182 F55, Gr.2
ASTM A 240 S31254, Gr.2
ASTM A 240 S31803, Gr.2
ASTM A 302 A & B
ASTM A 302 C
ASTM A 302 D

I would appreciate any kind of information.

Kindly regards,

ONE POINT












 
Replies continue below

Recommended for you

Hi,

The chemical and mechanical properties are indeed specified in the relevant ASTM sheets.
The minimum design temperatures for these materials are available in the relevant design code, e.g. such as the ASME B31.3 for piping. Material tables as listed herein specify the minimum (and maximum) design temperatures.

Success and regards,
FKE
 