Sep 1, 2003 #1 joeypanis Mechanical Joined Sep 1, 2003 Messages 2 Location US What material do you recommend for padeyes as per industry standard?
Sep 2, 2003 #2 jieli77479 Industrial Joined Aug 28, 2002 Messages 1 Location US AMTS A572-50 OR ASTM A516-70 Upvote 0 Downvote
Sep 2, 2003 #3 boo1 Mechanical Joined Oct 31, 2001 Messages 2,129 Location US Depends on you loading and allowable configuration. Upvote 0 Downvote
Sep 5, 2003 Thread starter #4 joeypanis Mechanical Joined Sep 1, 2003 Messages 2 Location US Thank you very much for the help. I'll be using ASTM572-50 for my 10 ton padeye to be used in an offshore rig. Upvote 0 Downvote
Thank you very much for the help. I'll be using ASTM572-50 for my 10 ton padeye to be used in an offshore rig.