I need to find all thread rod with a tensile strength between 90-110 ksi. I've contacted a few steel houses and can't seem to find anything in their inventory. Is there a material spec. that is around grade 70 with a UTS of 90-110 ksi? The rod sizes are 1/2".

Thanks,
M
 
F1554 grade 105 all thread rod. Look at other anchor bolt ASTM's as well.
 
Sorry, that's 105 yield, 125-150 UTS. Should get you started.
 
metalamn8357,

1/2" all thread rod is widely available in ASTM A193 gr.B7 (125ksi UTS/105ksi YTS) or gr.B7M (100ksi UTS/80ksi YTS).

Best regards,
Terry
 