arksurat
Mechanical
- Jan 30, 2002
- 9
I am making a pressure vessel as per ASME VIII div I for
crude oil seperator. My design pr/temp are 1440 psi / 100 DegC.
Shell material: 32mm thick, A 516 gr70 plate.
If I procure normalised plate, is it required to carry out
any SR / normalising after rolling prior to welding?
Is it mandatory as per code to order ultrasonically tested plate?
If so, as per which ASME standard (A435 / A577 / A578)?
Piping Material : API 5L X52 grade
As per API there are 2 classes PSL1 and PSL2.
Which class is required for my application?
crude oil seperator. My design pr/temp are 1440 psi / 100 DegC.
Shell material: 32mm thick, A 516 gr70 plate.
If I procure normalised plate, is it required to carry out
any SR / normalising after rolling prior to welding?
Is it mandatory as per code to order ultrasonically tested plate?
If so, as per which ASME standard (A435 / A577 / A578)?
Piping Material : API 5L X52 grade
As per API there are 2 classes PSL1 and PSL2.
Which class is required for my application?