kantipacific
Mechanical
Dear Group,
I just joined the group and am looking for your in material selection (cost and performance balance).
Application: Planetery gear train.
Can you please suggest which case is best suitable for gears:
1) 40Cr (AISI 5140) alloy steel gears with HRC 45-50
2) AISI 4140 Cr-Mo alloy steel gear with HRC 46-48
3) SCM415 (AISI 4115 or OLD SCM21)Cr-Mo steel case hardened to HRC 55-58
4) AISI 4340 Ni-Cr-Mo steel HRC 46-48 (I think this might be a overkill?)
Thank you
I just joined the group and am looking for your in material selection (cost and performance balance).
Application: Planetery gear train.
Can you please suggest which case is best suitable for gears:
1) 40Cr (AISI 5140) alloy steel gears with HRC 45-50
2) AISI 4140 Cr-Mo alloy steel gear with HRC 46-48
3) SCM415 (AISI 4115 or OLD SCM21)Cr-Mo steel case hardened to HRC 55-58
4) AISI 4340 Ni-Cr-Mo steel HRC 46-48 (I think this might be a overkill?)
Thank you