I have designed and built a pneumatic valve (current quantity four) with a G2 cast iron body and spool made of S7(Rc 50) with a lapped 45* seat and a land width of .125". It is used to control a circuit handling 250 psi for a valve gated hot runner.
Is this a good material selection for the body and spool?
I am considering using Dura-Bar 65-45-12 Ductile Iron
in replacement of the G2 for ease of manufacture but am concerned with the life of the seat.
Any suggestions?
Is this a good material selection for the body and spool?
I am considering using Dura-Bar 65-45-12 Ductile Iron
in replacement of the G2 for ease of manufacture but am concerned with the life of the seat.
Any suggestions?