Hi, All,
The elevated flare has a liquid seal drum at bottom, stack, and flare tip.
95 m high total, drum diameter is 3.6 m, stack diameter is 1.7 m.
If the design temperature is 425 C degree, design pressure is 5 barg for seal drum and stack, does SA-516 Gr.70N still work because the creep concerns. As per ASME STS-1, SA-242 is recommended at this temperature for stack, but can we use SA-242 for drum, pressure vessel?
SS304 could be selected, but the cost will be much higher.
Any recommendations on the material selection are very appreciated.
Sam
The elevated flare has a liquid seal drum at bottom, stack, and flare tip.
95 m high total, drum diameter is 3.6 m, stack diameter is 1.7 m.
If the design temperature is 425 C degree, design pressure is 5 barg for seal drum and stack, does SA-516 Gr.70N still work because the creep concerns. As per ASME STS-1, SA-242 is recommended at this temperature for stack, but can we use SA-242 for drum, pressure vessel?
SS304 could be selected, but the cost will be much higher.
Any recommendations on the material selection are very appreciated.
Sam