Oct 28, 2014 #1 KMur Mechanical Joined Apr 27, 2007 Messages 40 Location AE Dear all, I have following data to select the Material for KO drum. H2s=0% temp= 60° C Pressure=85.3 barg Gas flow rate= 4090 m³/h water fow rate= 0.6 m³/h This is sweet service. Please suggest me in selecting material of construction. thanks to all
Dear all, I have following data to select the Material for KO drum. H2s=0% temp= 60° C Pressure=85.3 barg Gas flow rate= 4090 m³/h water fow rate= 0.6 m³/h This is sweet service. Please suggest me in selecting material of construction. thanks to all
Oct 29, 2014 #2 cloa Petroleum Joined Jul 18, 2008 Messages 1,071 Location JP Don't double post http://www.eng-tips.com/threadminder.cfm?pid=1529Use translation assistance for Engineers forum Note the rules include No Student posting Upvote 0 Downvote
Don't double post http://www.eng-tips.com/threadminder.cfm?pid=1529Use translation assistance for Engineers forum Note the rules include No Student posting