Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material for Naphtha with 100 ppmw H2S

Status
Not open for further replies.

Novak11

Petroleum
Jun 16, 2014
6
Do you think it is OK to use Carbon steel with just 3 mm CA for Heat Exchanger for naphtha with content of 100 ppmw of H2S?
Thanks
 
Replies continue below

Recommended for you

It is naphtha stabilizer and temp. is 165 degC. In the meantime I checked couple of similar applications and found that all materials are really CS+3mm CA.
 