Apr 28, 2004 #1 mlh Mechanical Joined Aug 5, 2002 Messages 9 Location US What is the ASTM equivalent to CuSn5Zn5Pb Brass? Also, where can I find a chart that shows all of the material equivalents of metals?
What is the ASTM equivalent to CuSn5Zn5Pb Brass? Also, where can I find a chart that shows all of the material equivalents of metals?
Apr 28, 2004 1 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Regarding references, see the following thread: thread330-89970 I am not a copper expert, but this alloy appears to be similar to C54400 (88Cu-4Pb-4Sn-4Zn). You can perform your own cross-reference at http://www.copper.org Upvote 0 Downvote
Regarding references, see the following thread: thread330-89970 I am not a copper expert, but this alloy appears to be similar to C54400 (88Cu-4Pb-4Sn-4Zn). You can perform your own cross-reference at http://www.copper.org