What is the ASTM equivalent to CuSn5Zn5Pb Brass? Also, where can I find a chart that shows all of the material equivalents of metals?
 
Regarding references, see the following thread:

thread330-89970

I am not a copper expert, but this alloy appears to be similar to C54400 (88Cu-4Pb-4Sn-4Zn). You can perform your own cross-reference at
 