Nov 25, 2010 #1 Bozso Automotive Joined Nov 3, 2005 Messages 4 Location HU Hi, I have a drawing with material spec 12NC3 (CR1). I have found any data about 12NC3 (CR1) material. I am looking for material properties, equivalents. Thanks
Hi, I have a drawing with material spec 12NC3 (CR1). I have found any data about 12NC3 (CR1) material. I am looking for material properties, equivalents. Thanks
Nov 28, 2010 #2 ajack1 Automotive Joined Nov 24, 2003 Messages 1,148 Location GB I have no idea about 12NC3 but CR1 is cold rolled mild steel, I believe the German equivalent is St14 and the EN 10130 equivalent is DC04, but please check that. I would suggest contacting Corus. Upvote 0 Downvote
I have no idea about 12NC3 but CR1 is cold rolled mild steel, I believe the German equivalent is St14 and the EN 10130 equivalent is DC04, but please check that. I would suggest contacting Corus.