Hello all,
I am working on a project and having a bugger of a time finding a foundry that can help me match the material properties I am currently getting in a billet part. We are using 4340 and a custom heat treat recipe to get the following properties. Is there any way that these can be matched in a casting? Thanks in advance.
[ul]
[li]Yield 925MPa[/li]
[li]Ultimate 1080-1230 MPa[/li]
[li]Elongation 11%[/li]
[li]Charpy >35J @ -20C[/li]
[/ul]
I am working on a project and having a bugger of a time finding a foundry that can help me match the material properties I am currently getting in a billet part. We are using 4340 and a custom heat treat recipe to get the following properties. Is there any way that these can be matched in a casting? Thanks in advance.
[ul]
[li]Yield 925MPa[/li]
[li]Ultimate 1080-1230 MPa[/li]
[li]Elongation 11%[/li]
[li]Charpy >35J @ -20C[/li]
[/ul]