A detailed failure analysis of a 0.063" thick by 0.7" wide 17-7PH (Condition TH1050) flat torsion spring revealed two contributing factors: (1) scattered massive TiC particles that fractured, probably during cold reduction, leaving splits in the adjacent sound material; and (2) nearly continuous linear bands of ferrite, especially at the mid-thickness.
So my question: Is there any existing specification for 17-7PH that limits or even addresses the number or frequency or sizes of carbides?