I am having difficulty determining the cooling rate of the following application:
600 lbs of 1/4" x 4" steel pins (approx 7100 pins)
Cooling medium: Nitrogen at 15 psig
Gas recirculation at 5000 CFM
Initial load (pins) temp: 2000 deg F
Gas temp into load area: 150 deg F
The first issue I have is determining the final gas temperature as it leaves the load area to go into a heat exchanger. From this I will then need to size the heat-exchanger needed.
Can anyone recommend a solution to this problem.
Thank you
600 lbs of 1/4" x 4" steel pins (approx 7100 pins)
Cooling medium: Nitrogen at 15 psig
Gas recirculation at 5000 CFM
Initial load (pins) temp: 2000 deg F
Gas temp into load area: 150 deg F
The first issue I have is determining the final gas temperature as it leaves the load area to go into a heat exchanger. From this I will then need to size the heat-exchanger needed.
Can anyone recommend a solution to this problem.
Thank you