Hi guys,
I have a few defect issues that have surfaced on my job that I will be posting in the coming days so I hope you guys can help me out with them. First one:
I have a blockwall which was detailed to be tied into a stressed slab. A pour joint was provided to help mitigate some of the creep and shrinkage movement of the stressed slab, however it was still able to pull to block way which has resulted in some extensive cracking that I will need to "hide".
Can people please comment on the detailing I have provided, I think an ancon dowel or something that can allow some horizontal movmement would have been a much better detail. And a possible remedial method, I was thinking of providing a stainless steel cover plate which will allow any future movement while concealing the cracking. The client has suggested a saw joint (50mm) to initite a failure plane for any future cracking while repair the existing cracking which has occurred. Will a saw joint in blockwall only be effective if the block is cut before cracking occurs.
All comments will be appreciated.
I have a few defect issues that have surfaced on my job that I will be posting in the coming days so I hope you guys can help me out with them. First one:
I have a blockwall which was detailed to be tied into a stressed slab. A pour joint was provided to help mitigate some of the creep and shrinkage movement of the stressed slab, however it was still able to pull to block way which has resulted in some extensive cracking that I will need to "hide".
Can people please comment on the detailing I have provided, I think an ancon dowel or something that can allow some horizontal movmement would have been a much better detail. And a possible remedial method, I was thinking of providing a stainless steel cover plate which will allow any future movement while concealing the cracking. The client has suggested a saw joint (50mm) to initite a failure plane for any future cracking while repair the existing cracking which has occurred. Will a saw joint in blockwall only be effective if the block is cut before cracking occurs.
All comments will be appreciated.