Good day everybody,
We have carried out the visual inspection of 13%Cr pipes (L-80 13%Cr/AISI 420, API 5CT) and outcome had reveled rusty appearance on entire body. Upon asking, vendor informed that pipes were kept outside in open yard and due to unexpected raining; it was exposed and resulted in rusting (like black scale appearance) on external surface.
To know the genuine reason, what all can be instructed to vendor?
I have advised them to proceed with following steps:
1)PMI (positive material identification) to be carried out to know the chemical composition (13%Cr or not??)
2)Sweep blasting to be done to confirm bright & shiny appearance of surface
3)Coating to be applied on final product i.e. drilling cross-overs size: diameter 3-1/2” length 6 Ft
Do you have any suggestion any apart from above? And, also please can somebody suggest me on common appearance of 13%Cr steel (bright or??) AND
type of coating/painting applied on 13% Cr material?
Thanks in advance....
We have carried out the visual inspection of 13%Cr pipes (L-80 13%Cr/AISI 420, API 5CT) and outcome had reveled rusty appearance on entire body. Upon asking, vendor informed that pipes were kept outside in open yard and due to unexpected raining; it was exposed and resulted in rusting (like black scale appearance) on external surface.
To know the genuine reason, what all can be instructed to vendor?
I have advised them to proceed with following steps:
1)PMI (positive material identification) to be carried out to know the chemical composition (13%Cr or not??)
2)Sweep blasting to be done to confirm bright & shiny appearance of surface
3)Coating to be applied on final product i.e. drilling cross-overs size: diameter 3-1/2” length 6 Ft
Do you have any suggestion any apart from above? And, also please can somebody suggest me on common appearance of 13%Cr steel (bright or??) AND
type of coating/painting applied on 13% Cr material?
Thanks in advance....