We have some mechnical equipment operating right on the edge of shipping berths. An intitial paint system specified was as follows:
- Abrasive blast to SA 2 1/2.
- First coat inorganic zinc silicate. 70 - 85 um DFT.
- Second coat high build epoxy. 100 - 125 um DFT.
- Third coat high build epoxy. 100 - 125 um DFT.
Our customer has indicated they would like a top coat to retain its finish as long as possible. I have been recomended a urethane top coat by our paint supplier to replace listed top coat of high build epoxy. Said to provide good UV prtection and gloss retention.
Does this seem a reasonable system?
Dave
(also posted in "paint/coatings" forum)
We have some mechnical equipment operating right on the edge of shipping berths. An intitial paint system specified was as follows:
- Abrasive blast to SA 2 1/2.
- First coat inorganic zinc silicate. 70 - 85 um DFT.
- Second coat high build epoxy. 100 - 125 um DFT.
- Third coat high build epoxy. 100 - 125 um DFT.
Our customer has indicated they would like a top coat to retain its finish as long as possible. I have been recomended a urethane top coat by our paint supplier to replace listed top coat of high build epoxy. Said to provide good UV prtection and gloss retention.
Does this seem a reasonable system?