Mar 24, 2014 #1 khaled1973 Industrial Joined Mar 12, 2014 Messages 1 Location EG I ask about Marbel polishing powder composition
Mar 24, 2014 #2 bimr Civil/Environmental Joined Feb 25, 2003 Messages 9,380 Location US Marble polishing compound contains ingredients such as aluminum oxide, potassium oxalate, and shellac. The exact mixture will be a trade secret by the manufacturer. Upvote 0 Downvote
Marble polishing compound contains ingredients such as aluminum oxide, potassium oxalate, and shellac. The exact mixture will be a trade secret by the manufacturer.