Machinability and its minimal change when being heat treated. Thing of it is, is that we have been using it before we started using high speed machining therefore it was important to have minimal change. Now that we can high speed machine we almost don't need it but getting the Japanese higher ups to understand that is near impossible. Plus they make a fortune off of us as the Japan office buys from DAIDO then resells it to us. It sucks yes I know. Oh well.