any help here would be appreciated
I am interested in the amount of actual contraction after heat treat.
according to the material suppliers material data
the material contracts .001 in/in after aging.
Please advise if any one has actual experience with this material.
Thanks in Advance
I am interested in the amount of actual contraction after heat treat.
according to the material suppliers material data
the material contracts .001 in/in after aging.
Please advise if any one has actual experience with this material.