Manufacturer for GRP pipe?

Status
Not open for further replies.

Redpipe

Mechanical
Joined
Sep 17, 2002
Messages
17
Location
TH
Could you please help me?

Now I need to order GRP pipe and fitting for open drain lines in offshore.

I know only Ameron GRP pipe. I think that Ameron GRP pipe is expensive.

Anybody tell me other manufacturers?

Many thanks,

Bill
 
Star
Fibrespar
Smith
Futurepipe

There are many others.

Careful though, some products come from the downhole tubing industry and are very rugged, high pressure (and so expensive) while others come from the B31.3 piping industry and are less expensive. Some manufacturers do both (Star and Centron/Ameron) but in different factories.

The major manufacturers have manufacturing facilities spread around the world so the price will vary with where they were made. Dennis Kirk Engineering
 