The 3,5mm (10/2 - 3/2) of land either side of the root bevel on the lower face (in the diagram) may be difficult to achieve good fusion. As is often the case, if it presents a challenge to the welder, then it will present a challenge to the UT tech as well. Of course if the very best welders and UT techs in the country have been hired then this will mitigate the risk. If not, shear wave UT will not detect LOF in those areas I have highlighted.
Good luck.