magnetite coating to prevent rubber fouling

Status
Not open for further replies.

bikswahla

Mechanical
Joined
Oct 19, 2006
Messages
17
Location
US
group

Hope some one can help me in this, I was reading about rubber fouling in the forum and in the article it says a magnetite coating can prevent rubber fouling, we have a similiar issue in our process but I am not able to find any metal finishing company who can do " Magnetite coating" some of them never heard of this type of coating, my question is do any one of you know who can do this type of coating or is there any other name called for this kind of coating??

Thanks for the help
 
There is a company called "Magnaplate" that offers a variety of low friction or low wear coatings. Google the name and you should get their website.
 