I'm having trouble finding information regarding the magnetic properties of Hastelloy C276. Anybody know where I can look to find it? Thanks for any help.
 
Replies continue below

Recommended for you

Per Special Metals:
Permeability at 200 Oersted (15.9 kA/m.....1.0002

 