In M.4.2 for the shell to bottom joint we shall do as following:
"MT shall be performed at every 13mm of deposited weld metal while the weld is being made and on the completed weld."
if the bottom plate is 10mm thk. and first course shell is 12 mm the fillet weld size is smaller than 13mm, then is that necessary to perform MT as above?
generally, what is the meaning of
"MT shall be performed at every 13mm of deposited weld metal while the weld is being made and on the completed weld."
if the bottom plate is 10mm thk. and first course shell is 12 mm the fillet weld size is smaller than 13mm, then is that necessary to perform MT as above?
generally, what is the meaning of