Hello,

we have to use a chinese standard 20CrMn cast hardened steel. Can anyone provide us with the amgnetic material properties of this carbon steel?

This steel is a chinese standard, and we face problems on finding material properties. Unfortunately we have to use it, since the customer want to use only this steel!

thanks a lot

best regards
Ioannis
 
what is the composition? if it is equivalent to 304 austenitic stainless steel, it is non-ferromagnetic! magnetic properties make no sense.
 
Hello MagBen,


thanks for the reply. I guess it is not like the 304 steel. The 20CrMn is a case-hardened steel which magnetic properties are slightly different from the original 20CrMn material. In the application it is used, it has been reported that it has a residual magnetization. I need the material properties, the BH curve for simulating this magnetization effects.

thanks