Mar 16, 2020 #1 dougs1967 Mechanical Joined Jan 30, 2013 Messages 11 Location US Any suggestions where I can find the subject material for a special application. Volumes to be injection molded are in the area of 7-10K lbs. annually. Thanks
Any suggestions where I can find the subject material for a special application. Volumes to be injection molded are in the area of 7-10K lbs. annually. Thanks
Mar 16, 2020 #2 IRstuff Aerospace Joined Jun 3, 2002 Messages 44,942 Location US What exactly do you mean by "Magnetic Conductive Static Discharging Polypropylene" particularly the first part? Note that ESD polypropylene bags are mostly banned from most companies, for various reasons. TTFN (ta ta for now) I can do absolutely anything. I'm an expert! https://www.youtube.com/watch?v=BKorP55Aqvgfaq731-376 forum1529 Entire Forum list http://www.eng-tips.com/forumlist.cfm Upvote 0 Downvote
What exactly do you mean by "Magnetic Conductive Static Discharging Polypropylene" particularly the first part? Note that ESD polypropylene bags are mostly banned from most companies, for various reasons. TTFN (ta ta for now) I can do absolutely anything. I'm an expert! https://www.youtube.com/watch?v=BKorP55Aqvgfaq731-376 forum1529 Entire Forum list http://www.eng-tips.com/forumlist.cfm
Mar 17, 2020 #3 TugboatEng Marine/Ocean Joined Nov 1, 2015 Messages 12,177 Location US You can use carbon fiber to make the plastic conductive. Embed magnetic elements to make it magnetic. Upvote 0 Downvote
You can use carbon fiber to make the plastic conductive. Embed magnetic elements to make it magnetic.