I seem to remember that there is a type of bronze that is slightly magnetic . Is my memory correct ?
 
Replies continue below

Recommended for you

The only way perhaps is the iron content going above 5%(Please correct me).

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
There is an alloy that consist of Copper, Aluminum, Manganese that is very magnetic. If memory serves me well I think it's called Huesler's alloy.
 