scotteekay
Mechanical
Greetings. Working on a linear type solenoid. Have identified internal core component to be low carbon <.05, Mn .22 P, .011... HRB 27-37. Material identifes as AISI 1005, 1006. I am having trouble locating bar stock to make prototype samples, and to secure a production source. Does anyone have a source? or might reccomend an alternate more commercially available material? We have had some luck with 12L14, but variations in carbon up to .15 may give is some performance issues. Any input would be appreciated.
Scott
Scott