Having a problem with corrosion showing up on ZE41A-T5 magnesium cast housings. Parts are coated with Dow 17 (with the exception of Dow 7 or Dow 19 on some drilled areas). A top layer of Rockhard PT961 is applied over most of the Dow 17 areas. Parts are coated with a cosmoline material, and securely packaged with dessicant. After as little as one month of storage, Widespread corrosion shows up on areas that were machined. Corrosion Most notable on areas that only received Dow 17 but it is also seen coming up from areas that received Rockhard, causing the Rockhard to peel. Any ideas as to what could be causing this?