Nov 26, 2003 #1 braze Automotive Joined Jul 24, 2003 Messages 1 Location GB Can anyone point me in the right direction with regards to getting material "Mag Perm Tested"?
Can anyone point me in the right direction with regards to getting material "Mag Perm Tested"?
Nov 26, 2003 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US What type and form of materials are you looking for? Is the magnetic permeability of any metal or do you a specific magnetic permeability? Upvote 0 Downvote
What type and form of materials are you looking for? Is the magnetic permeability of any metal or do you a specific magnetic permeability?
Nov 27, 2003 #3 hacksaw Mechanical Joined Dec 7, 2002 Messages 2,587 Location US it is a variation of eddy current testing (NDT) and used to identify regions of high local stress. Upvote 0 Downvote
Nov 28, 2003 #4 JSMAT Materials Joined Jan 15, 2003 Messages 5 Location GB The test is pretty straightforward, a number of commercial test labs could do it on a sample or 'on site' Try mailto:cts@allvac.co.uk if you're in the UK Upvote 0 Downvote
The test is pretty straightforward, a number of commercial test labs could do it on a sample or 'on site' Try mailto:cts@allvac.co.uk if you're in the UK