Hello:

I frequently see the terms “macro” and/or “micro” on material certification reports. What do these terms mean?

Are these terms related to a UT inspection?

Thanks in advance for the help,
Fracball
 
They refer to optical examination of the material
Macro usually refers to examinations at magnifications up to about X10
Micro refers to examinations at higher magnifications - typically around x400.
 
Macro is a term used to define magnification of 10X or less. Micro is used for maginification >10X, (typically 100X or more.)
 