Apr 1, 2004 #1 Fracball Mechanical Joined Aug 21, 2002 Messages 10 Location US Hello: I frequently see the terms “macro” and/or “micro” on material certification reports. What do these terms mean? Are these terms related to a UT inspection? Thanks in advance for the help, Fracball
Hello: I frequently see the terms “macro” and/or “micro” on material certification reports. What do these terms mean? Are these terms related to a UT inspection? Thanks in advance for the help, Fracball
Apr 1, 2004 #2 Carburize Materials Joined Sep 23, 2002 Messages 702 Location US They refer to optical examination of the material Macro usually refers to examinations at magnifications up to about X10 Micro refers to examinations at higher magnifications - typically around x400. Upvote 0 Downvote
They refer to optical examination of the material Macro usually refers to examinations at magnifications up to about X10 Micro refers to examinations at higher magnifications - typically around x400.
Apr 1, 2004 #3 CWIC Specifier/Regulator Joined Feb 14, 2003 Messages 245 Location US Macro is a term used to define magnification of 10X or less. Micro is used for maginification >10X, (typically 100X or more.) Upvote 0 Downvote
Macro is a term used to define magnification of 10X or less. Micro is used for maginification >10X, (typically 100X or more.)