Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Macro & Micro Tests?

Status
Not open for further replies.

Fracball

Mechanical
Aug 21, 2002
10
Hello:

I frequently see the terms “macro” and/or “micro” on material certification reports. What do these terms mean?

Are these terms related to a UT inspection?

Thanks in advance for the help,
Fracball
 
Replies continue below

Recommended for you

They refer to optical examination of the material
Macro usually refers to examinations at magnifications up to about X10
Micro refers to examinations at higher magnifications - typically around x400.
 
Macro is a term used to define magnification of 10X or less. Micro is used for maginification >10X, (typically 100X or more.)
 