As a "general rule" and not so specific to a type of rubber compound. What would be some methods of machining in a lathe? Cut Vs Grind, how do higher or lower work speeds affect the finish?
What I have is a vulcanized roller with a pitted and uneven surface. My plan is to remove some of the surface and make it usable again. ANY input is appreciated.