Hi all
When machining Round tensiles to ASTM A370 Fig 5 specimen 4 is the metric 12.5mm size a standalone size and NOT a conversion from the imperial 0.500" quoted.
what is the reason for this not being 12.70mm ?

L.E.B1
 
Replies continue below

Recommended for you

The answer is proportions. There is a 1.6% difference between the English and metric diameters for these specimens. This is the same percentage difference between the 50.8 mm gage length of a 2" specimen and the 50 mm metric length that is actually specified. The difference is to maintain specimen proportions while maintaining easily defined dimensions.

Aaron Tanzer
 
Simply put, Codes and Standards typically rely on soft conversions between SI and US customary units.
 
Hi Leb1,
I think that in all ASTM standards there is a sort of 'warning' in the 1st section of the standard. This 'warning' concerns units conversion between imperial and metric