Hello,
I had simulated a core (low carbon steel 1008) wound with Cu wire in Ansys magnetostatics. An armature (permanent magnet in this case) placed in a gap of the core was simulated to calculate forces.
However the force I am getting from an actual machined 1010 steel core is significantly less (more than factor of 2).
Why is this happening? Is this due to stress formed by machining that could be affecting the grain structure? Should I look into annealing/plating with high permeability mat? please help !